Working process and cold brittleness of high precision cold drawn tube

Jul 03, 2019

Leave a message

The cold brittleness (or low-temperature embrittlement tendency) of the high precision cold drawn tube is expressed by the toughness-brittle transition temperature Tc. High purity iron (0.01% C) has a Tc at 100 C. Below this temperature, it is completely in an embrittled state. Most alloying elements in cold-rolled precision bright steel tubes increase the toughness-brittle transition temperature of cold-rolled precision bright steel tubes, increasing the tendency of cold and brittleness. When the ductile fracture occurs above room temperature, the fracture of the cold-rolled precision bright steel pipe is a dimple-type fracture, and the fracture is a cleavage fracture at a low temperature.

The factors that increase the cold brittleness of cold-rolled precision bright steel pipes are: (1) solid solution strengthening elements. Phosphorus increases the toughness and brittleness of the transformation temperature; there are also molybdenum, titanium and vanadium; the elements with low content and low content and high toughness and brittle transformation temperature are silicon, chromium and copper; reducing toughness and brittle transformation There is nickel at the temperature, and manganese is reduced first and then increased toughness and brittle transition temperature. (2) An element forming the second phase. In the second phase, the important element of the cold-rolled precision bright steel tube is carbon, and the carbon content in the cold-rolled precision bright steel tube increases. The pearlite content in the cold-rolled precision bright steel tube increases, and the average pearlite volume increases by 1%. A brittle transition temperature increased by an average of 2.2 °C.

www.skivingtubelw.com

Send Inquiry