Embrittlement of precision steel pipe

Apr 02, 2020

Leave a message

After the austenitic mechanism is obtained from the ultra-low temperature quenching of the brittle fracture alloy steel for precision steel tube, the steel is embrittled in the temperature range of 250-400 ℃, and its ductility brittle fracture transition temperature rises significantly. The embrittled precision steel pipe of seamless steel pipe can not be removed by ultra-low temperature quenching and heating, so it is also called% 26ldquo; irreversible quenching brittle fracture% 26rdquo;. Its key products are alloy tool steel and alloy structural steel such as low alloy high compressive strength precision pipe. The fracture of seamless steel tube is intergranular fracture or intergranular and quasi cleavage mixed fracture. It is widely believed that the cause of brittle fracture in ultra-low temperature quenching is as follows:

(1) It is closely related to the fact that the cementite dissolves at the grain boundary of the original ferrite in the form of thick sheet during the ultra-low temperature quenching, leading to the grain boundary embrittlement.

(2) One of the reasons for the brittle fracture is the segregation of the residual phosphorus at the grain boundary of the ferrite. The high purity precision steel pipe with phosphorus content less than 0.005% does not cause brittle fracture in ultra-low temperature quenching. When phosphorus is heated by fire, ferrite grain boundary segregation occurs, which is preserved after heat treatment. The segregation of phosphorus at the grain boundary of the ferrite and the dissolution of phosphorus at the grain boundary of the ferrite during the cementite quenching lead to intergranular embrittlement and promote the generation of brittle fracture in the ultra-low temperature quenching.

The aluminum alloy element in precision steel tube is harmful to the brittle fracture of ultra-low temperature quenching. Chromium and manganese promote the segregation of residual phosphorus at ferrite grain boundaries, and then promote the brittle fracture of ultra-low temperature quenching. Most of tungsten and vanadium are harmless. Molybdenum can reduce the ductile brittle fracture transition temperature of ultra-low temperature quenching precision tubes, but it can not prevent the brittle fracture of ultra-low temperature quenching. Silicon can delay the dissolution of cementite during quenching and increase its conversion temperature, so it can increase the temperature of brittle fracture of precision steel tube during ultra-low temperature quenching.


Send Inquiry